logo
  • English
Home ProductsFerro Titanium

Good Quality Used In Steel Making Titanium Iron FTi35 FTi35 FeTi70% Ferro Titanium

I'm Online Chat Now

Good Quality Used In Steel Making Titanium Iron FTi35 FTi35 FeTi70% Ferro Titanium

Good Quality Used In Steel Making Titanium Iron FTi35 FTi35 FeTi70% Ferro Titanium
Good Quality Used In Steel Making Titanium Iron FTi35 FTi35 FeTi70% Ferro Titanium
Good Quality Used In Steel Making Titanium Iron FTi35 FTi35 FeTi70% Ferro Titanium Good Quality Used In Steel Making Titanium Iron FTi35 FTi35 FeTi70% Ferro Titanium Good Quality Used In Steel Making Titanium Iron FTi35 FTi35 FeTi70% Ferro Titanium Good Quality Used In Steel Making Titanium Iron FTi35 FTi35 FeTi70% Ferro Titanium Good Quality Used In Steel Making Titanium Iron FTi35 FTi35 FeTi70% Ferro Titanium

Large Image :  Good Quality Used In Steel Making Titanium Iron FTi35 FTi35 FeTi70% Ferro Titanium

Product Details:
Place of Origin: China
Brand Name: ZHENAN
Certification: ISO9001:2015
Model Number: Ferro Titanium
Payment & Shipping Terms:
Minimum Order Quantity: Negotiable
Price: Negotiable
Packaging Details: 1MT big bag or as per customer request
Delivery Time: 7-10 work days after received the payment
Payment Terms: L/C, T/T, Western Union
Supply Ability: 2000MT/per Month

Good Quality Used In Steel Making Titanium Iron FTi35 FTi35 FeTi70% Ferro Titanium

Description
Product Name: Ferro Titanium Color: Silver Gray
Model: Ti,C,S,P,Si,Al,Mn, Ti,C,S,P,Si,Al,Mn Shape: Block/lump
Package: 1 Mt Bag Application: Steelmaking, Casting,Welding Materials
Highlight:

Good Quality Ferro Titanium

,

FeTi70% Ferro Titanium

,

Steel Making Ferro Titanium

Good Quality Used in Steel Making Titanium Iron FTi35, FTi35, FeTi70% Ferro Titanium

 ferrotitanium 


Analysis of Factors Affecting Ferrotitanium Smelting


Abnormal Phenomena in Ferrotitanium Smelting

 

Moisture in the charge causes boiling, uneven gas escape, and excessive material ejection. The use of magnesite containing moisture for sand holes can also lead to material ejection.


Non-uniform mixing of the charge results in uneven smelting.


Low unit heat input leads to slow reactions, prolonged smelting time, insufficient reductant, low heat generation, or low preheating temperature of the charge, resulting in a cold process. This can cause excessive slag adhesion at the bottom of the ingot, high iron content in the slag, poor fusion of the ingot, looseness, or slag inclusions.


High unit heat input or high preheating temperature results in violent reactions, slag agitation, slag splashing, hard and difficult-to-break ingots, high aluminum content in the ingots, and reduced yield.

 

 

Specifications 


 

 

Ferro titanium specification
Grade Ti Al Si P S C Cu Mn
FeTi30-A 25-35 8.0 4.5 0.05 0.03 0.10 0.2 2.5
FeTi30-B 25-35 8.5 5.0 0.06 0.04 0.15 0.2 2.5
FeTi40-A 35-45 9.0 3.0 0.03 0.03 0.10 0.4 2.5
FeTi40-B 35-45 9.5 4.0 0.04 0.04 0.15 0.4 2.5
FeTi70-A 65-75 3.0 0.5 0.04 0.03 0.10 0.2 1.0
FeTi70-B 65-75 5.0 4.0 0.06 0.03 0.20 0.2 1.0
FeTi70-C 65-75 7.0 5.0 0.08 0.04 0.30 0.2 1.0
Size 10-50mm
60-325mesh
80-270mesh & customerize size

 

 

Good Quality Used In Steel Making Titanium Iron FTi35 FTi35 FeTi70% Ferro Titanium 0

 

Packing & Delivery


 

Packing: 1 ton big bag, 20-25mt in 20' container

 

Ferro Silicon Magnesium Ferro Silicon Lump  Ferro Silicon Metal Products

 

Company Profile


ZHENAN has been in the business of ferroalloy for 30 years now. It is a leading manufacturer and supplier of ferro silicon,silicon manganese,silicon metal,silicon carbide,high carbon silicon and so on.our company is a large-sized production enterprise integrating research, development, production and sales.

 

Our Services


Q:Can we visit your factory ?
A:Warmly welcome once we have your schedule we will pick you up .

 

Q: Do you have quality control?
A: Yes, we have gained BV, SGS authentication.


Q: How long is your delivery time?
A: Generally it is 7-14 days if the goods are in stock. or it is 25-45 days if the goods are not in stock, it is according to
quantity.


Q:Can we get the some samples?Any charges?
A: Yes , we could offer the sample for free charge but do not pay the cost of freight . If you place the order after confirm the sample , we will refund your express freight or deducte it from the order amount .

Contact Details
Zhenan Metallurgy Co., Ltd

Contact Person: Mr. xie

Tel: + 8615896822096

Fax: 86-372-5055135

Send your inquiry directly to us (0 / 3000)