Product Details:
|
Color: | Silver | Density: | 10.22 G/cm3 |
---|---|---|---|
Hs Code: | 81019500 | Payment Term: | T/T, L/C, Etc. |
Process: | Cold Rolled,hot Rolled,riveting | Technique: | Power Metallurgy |
Highlight: | 10.22 g/cm3 tzm material,customized tzm material |
ZhenAn stocks TZM Molybdenum (Titanium Zirconium Molybdenum) in a variety of forms and sizes. Below are most of the standard stock forms/sizes. If you don't see the size or shape of TZM Molybdenum (Titanium Zirconium Molybdenum) that you need, please call one of our material specialists; our knowledgeable sales staff can help you. We can cut, slit, shear or center-grind TZM molybdenum materials to your specifications, and we offer great flexibility in custom sizes, packaging and special materials!
TZM alloys (titanium-zirconium-molybdenum) have a finer grain structure. TiC and ZrC formed in the molybdenum grain boundaries suppress grain growth and inhibit base metal failure due to fracture along the grain boundaries. TZM alloys cost about 25 percent more than pure molybdenum, but processing costs are only about 5-10 percent higher. For high-strength applications such as rocket nozzles, structural parts for furnaces and forging dies, the cost difference of this alloy is worthwhile.
TZM molybdenum is available in sheet and bar form in essentially the same size range as molybdenum, with the exception of thin foils, and Rembar has extensive experience in the manufacture of TZM alloys (titanium-zirconium-molybdenum). Please refer to the separate TZM table.
TZM molybdenum and molybdenum alloys have high recrystallization temperatures, high heat resistance and good creep properties.
Translated with www.DeepL.com/Translator (free version)
TZM alloy (molybdenum zirconium-titanium alloy) and physical properties of pure molybdenum compared as follows:
Material |
density /g·cm-3 |
Melting point /℃ |
Boiling point /℃ |
TZM alloy (Ti0.5/Zr0.1) |
10.22 |
2617 |
4612 |
Mo |
10.29 |
2610 |
5560 |
Mechanical Properties of TZM alloy (molybdenum zirconium-titanium alloy) (ri0.5 / Zr0.1) as follows:
Mechanical Properties |
Elongation (%) |
elasticity modulus GPa |
Tensile strength Mpa |
yield strength Mpa |
fracture toughness MP·m1/2) |
Value |
<20 |
320 |
685 |
560-1150 |
5.8-29.6 |
TZM alloy (molybdenum zirconium-titanium alloy) high-temperature tensile strength and elongation:
Temperature |
tensile strength(Mpa) |
Elongation |
RT |
1140-1210 |
7.5-13.0 |
1000 |
700-720 |
5.2 |
1200 |
320-360 |
9.0 |
1300 |
190-210 |
11.5-13.5 |
1400 |
140-170 |
11-16 |
TZM alloy (molybdenum zirconium-titanium alloy) thermal performance and electrical properties:
Performance |
coefficient of thermal expansion /K-1(20~100℃) |
thermal conductivity W/m·K |
Using maximum temperature in air ℃ |
ResistivityΩ·m |
Value |
5.3X10-6 |
126 |
400 |
(5.3~5.5)X10-8 |